Record Weight Anodized CNC Machining Aluminum Parts
Jun 26, 2014
Leave a message
Reduce the service life of the mold: due to the high hardness of the oxide scale, the oxide scale in the mold cavity will accelerate the wear of the mold cavity, thereby reducing the service life of the mold and also affecting the service life of the machining tool. The oxide scale (alkaline) peels off on the bottom of the furnace, and it reacts with the refractory material (acidic) at the bottom of the furnace to make the bottom of the furnace reflow and shorten the service life of the heating furnace. Increase the scale removal process: not only the scale removal process is required in the production process of the wheel forgings, but also the shot blasting, sandblasting or pickling process of the wheel forgings.