If there are defects such as cracks, folds, forgings, interlayers, scars, slag inclusions, etc., on the surface of the wheel forgings, the following regulations shall be implemented:
For the surface of the forging that needs to be machined, the defect depth is confirmed after inspection, and it can be guaranteed that more than 50% of the machining allowance is left. It is allowed not to be removed, but the user's consent is required